Hey Art, As you would suspect, adding old paste to new paste is a ratio game. If you have a half jar of old paste and a half jar of new paste, and you mix them, then the new mixture is better than the old paste, but not as good as new paste. For practical help, the rule of thumb that I prefer is that you should never put old/used paste into a jar with new/unused paste. When you are done with the build, or done for the day, the used and unused paste should be kept in separate containers. At least in my humble opinion. If you have solder paste on the stencil, and the amount depletes to a level in which you need to add paste, I have no problem with mixing in new paste. This will improve the condition of solder paste on the stencil. Perhaps this is what your coworker is talking about. Steve A > -----Original Message----- > From: Surface Mount [SMTP:[log in to unmask]] > Sent: Thursday,February 07,2002 1:48 PM > To: [log in to unmask] > Subject: [TN] > > Hello, > > I work for a small PCB Manufacturing plant in Michigan. I am somewhat > new to the buisness, and my co-workers have been giving me info about > solder > paste, but there seems to be some questions about solder paste use > We use Kester R562 solder paste. One of the things they are telling me is > mixing new solder paste with old solder paste will rejuvinate the old > paste. > Is this true, or will it just ruin the new paste. > > Art Hampton > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------