Hi Doug, We use a Master Bond product, UV15-7TK1A, For staking wires (all aerospace). This adhesive is UV curable (30 seconds), solvent resistant and doesn't run. The down side, it's somewhat expensive, hundreds of dollars for a quart can. It lasts a long time, though, even though the shelf life is six months, we keep on extending it as long as it meets the hardness requirement after cure. Haven't had any problems with adhesive that was over 2 years old, but scraped it anyway, why push your luck. Been using this stuff for 6 or 7 years. Jim Marsico Senior Engineer Production Engineering EDO Electronics Systems Group [log in to unmask] <mailto:[log in to unmask]> 631-595-5879 -----Original Message----- From: [log in to unmask] [SMTP:[log in to unmask]] Sent: Monday, January 07, 2002 2:41 PM To: [log in to unmask] Subject: [TN] Staking compounds Good day all, I am curious as to what all y'all use for staking compounds (to fix wires or components in place) on your assemblies, especially if you are in the high-rel area or aerospace sector. Thanks. Doug Pauls Rockwell Collins ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------