Yep! Our assmebly house bakes the boards for about 3 hours at 90 deg C to dry them out after a wash. Peter Warren_Crow@I -O.COM To: [log in to unmask] Sent by: cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST TechNet Aero/ST Group) <[log in to unmask] Subject: [TN] Baking of Assemblies? ORG> 01/19/02 05:03 AM Please respond to "TechNet E-Mail Forum."; Please respond to Warren_Crow This should be good fodder! We wash PWAs in a water hurricane type machine, with a hot air blower at the end of cycle. We noticed some components mainly elect. alum. capacitors have high capacitance. After research on cap. we were instructed to bake assemblies 20 mins @ 100c to dry them. The long term effect of the moisture in the cap would cause electrical leakage then failure due to corrosion. Well this idea expanded into a question should we bake all assemblies because many other items such as transformers, pots., coils are not hermetically sealed. And then there is the issue with pwb material its self. My question to the forum is, Does anyone bake after wash as a standard? All points of view are welcome. Thanks! --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- [This e-mail is confidential and may also be privileged. If you are not the intended recipient, please delete it and notify us immediately; you should not copy or use it for any purpose, nor disclose its contents to any other person. Thank you.] --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------