You can go to there web sight a thttp://www.4taconic.com/index.htmln This should help you and they have been very helpful on issues on material I have had in the past "Tempea, Ioan" <itempea@POSIT To: [log in to unmask] RON.QC.CA> cc: Sent by: Subject: [TN] Taconic teflon TLX-8 TechNet <[log in to unmask] RG> 01/14/02 09:53 AM Please respond to "TechNet E-Mail Forum." Hi technos, please give me a hint on what Taconic Teflon TLX-8 is and it's solderability properties. I saw this specified on an RF drawing and I wonder if it can be reflowed. Any other concerns? Also, any directions towards an on-line resource would be highly appreciated. Thanks, Ioan --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------