Dan, Can't thank you enough. I'm sure Peter thanks you as well. His problems seems a bit different with the Ni finish. Any suggestions? The German silver thing occurred using shields on R/F filters. It happened several times so I contacted someone at HAC and they recommended the "pink death" flux that did the job but not without regrets. Thanks again, Earl Moon --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------