Why would
anyone think that 100% touch up would be effective?
In my
experience touch up is likely to cause more problems than it solves - if you
must do it and the application is that critical then I would say go automatic
as you will have direct control of soldering parameters
Neil
-----Original
Message-----
From: Becerra Alejandro
[mailto:[log in to unmask]]
Sent: 05 December 2001 02:19
Subject: Manual Soldering vs.
Automatic Soldering
Hello to All,
One product request a
100% touch up in several joints because of safety.
We are considering doing this process by manual
soldering or using automatic soldering (robot).
What are the advantage and disadvantage of both
procedures?
Where can I find a comparison between them?
Is there any reliability issue in using manual
soldering?
Any help will be greatly
appreciated
Alejandro Becerra