Doug and Jim In respect to the suggestions Doug makes, could you just be sure that you are manufacturing assemblies that are broadly in-line with the "coupon design" outlined in J-Std001/004/TM650 etc.. Latest research suggests that "older" designs might yield grossly misleading reliability data (SIR results) - you really must test to conditions to which your finished assembly shall be subjected. "Cleaning" to a value of less than 2 megohm/cm also means that it is acceptable to leave up to that amount of "salt" on every square cm of the assembly, but fine-line; fine-pitch; COB, BGA etc., might well demand a far lower value. I know of many that work to less than 0.2 megohm/cm for this very reason. Regards, Graham Naisbitt [log in to unmask] www.concoat.co.uk <http://www.concoat.co.uk> For instant access to Product Data Sheets register on the Tech-Shot area of http:// www.concoat.co.uk <http://www.concoat.co.uk> Concoat Limited Alasan House, Albany Park CAMBERLEY GU16 7PH UK Phone: +44 (0)1276 691100 Fax: +44 (0)1276 691227 Mobile: +44 (0)79 6858 2121 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask] Sent: Monday, December 10, 2001 02:12 To: [log in to unmask] Subject: Re: [TN] Conformal Coating Process I'm trying to qualify a new cleaning process for electrical assemblies prior to conformal coating (Military boards). The old MIL Specs had as cleanliness requirement of 2 meg-ohms minimum, is this all I need to do, verify cleanliness to 2 meg-ohms? What about subjecting the assemblies to 10-day elevated temp/humidity (steady state)? Any recommendations? *Jim, to your first question, Yes. When changing a cleaning operation, and not changing fluxes, MIL-STD-2000A only required Appendix C testing, which was the standard ROSE test. The 2 megohm-cm requirement translates to the more familiar 10.06 micrograms sodium chloride equivalence per square inch, whatever that becomes translated to the specific ionic cleanliness tester. We all know what a crock that test is, but it still exists, especially in military contracts. Two questions you should be asking: What data does my customer need to see? and I just trying to meet contractual requirements or REALLY show that the change is not detrimental? If the customer leaves it totally to you, then I suggest that you do both. The ROSE test, bogus as it may be, is very easy to do and satisfies the contractually focussed types. As to a longer temperature-humidity exposure, that is a fairly good idea. What tests to you perform now to tell you if product is good or bad? Do that same test but extend the test time about 50% and run on hardware cleaned with the new method. At Collins, our products go through -55 to 125C cycling to catch infant mortality types of failures, er...ahhh... not that we EVER see such failures, mind you....., and when we have a process change, we use the same environmental screen. Doug Pauls Rockwell Collins ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------