The profile for removal does not need to be as long as the profile for replacement. But it won't hurt to use a good replacement profile to remove the part. > -----Original Message----- > From: TechNet [mailto:[log in to unmask]]On Behalf Of David Fish > Sent: Wednesday, November 07, 2001 8:21 PM > To: [log in to unmask] > Subject: Re: [TN] BGA rework - part removal profile > > > Look here: http://developer.intel.com/design/Quality/component/rework.htm > > Dave Fish > ----- Original Message ----- > From: "Andrew Chansler" <[log in to unmask]> > To: <[log in to unmask]> > Sent: Wednesday, November 07, 2001 1:58 PM > Subject: [TN] BGA rework - part removal profile > > > > Should I use the same thermal profile (the one used for reflow) > to remove > a > > BGA for rework? or I need a different profile specifically for part > > removal? > > > > Thanks, > > AC > > > > > -------------------------------------------------------------------------- > ------- > > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > > To unsubscribe, send a message to [log in to unmask] with > following text in > > the BODY (NOT the subject field): SIGNOFF Technet > > To temporarily halt delivery of Technet send the following message: SET > Technet NOMAIL > > Search previous postings at: www.ipc.org > On-Line Resources & > Databases > > E-mail Archives > > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > > > -------------------------------------------------------------------------- > ------- > > > > ------------------------------------------------------------------ > --------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following > message: SET Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & > Databases > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ------------------------------------------------------------------ > --------------- > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------