Hi Rudy! Sorry, I was just thinking about the three immersion silver finishes I have worked with - you are correct, there are several other immersion silver finishes available on the market. My big confusion was the term "organic" silver - is there two types of immersion silver finishes: organic versus metallic? Or is the use of the term "organic" describing some of the codeposited constituents of an immersion silver finish? Dave Hillman Rockwell Collins [log in to unmask] "<Rudy Sedlak>" <[log in to unmask]>@ipc.org> on 11/28/2001 06:56:39 PM Please respond to "TechNet E-Mail Forum." <[log in to unmask]> Sent by: TechNet <[log in to unmask]> To: [log in to unmask] cc: Subject: Re: [TN] Organic Silver PCB's Ahem, Sir Dave: How many immersion Silver systems did you say there were? Ever heard of SilveR ShielD? Do the capitolized last letters of the name give you a hint? Rudy Sedlak RD Chemical Company --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------