I have always seen fairly good wetting of immersion silver PCBs and whilst they may not be as good as HASL this is usually only evident on the lack of wetting to the outer edges of lands on the topside of PTH boards and less fill on larger hole sizes. I have certainly never seen anything like you are describing. My first question would be what flux are you using? 160degC topside temperature after preheat sounds very hot (regardless of finish) and it may be that a problem with your profile is more evident on the immersion silver boards. Regards, Neil Atkinson -----Original Message----- From: Michael Bell [mailto:[log in to unmask]] Sent: 28 November 2001 19:00 Subject: Organic Silver PCB's Hi there Technetters, I have now exhausted my efforts of improving the solderability (T/H) of some RF Organic Silver PCB's we are currently making. Every attempt to improve the solderability has had no impact. The soldered PCB's show very poor wetting, partial joints and in some areas there is no evidence of solder. The PCB is curretly being pre-heated to around 160 deg. C topside and a bath temperature of 256 deg. C. Is there something I am over looking with the Organic Silver? Is there any special method/ or profile for Organic SIlver finished PCB's??? Any feedback would be appreciated. Cheers Mike _____________________________________________________________________ This message has been checked for all known viruses by Star Internet delivered through the MessageLabs Virus Scanning Service. For further information visit http://www.star.net.uk/stats.asp or alternatively call Star Internet for details on the Virus Scanning Service. --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------