Bev, How come you are soldering those wires to cans anyhow. I thought those new fangled communication devices used the strings. P.S. I think it's the flux activity level that supports elements that have surface oxidation issues. My handy dandy Kester flux selector slide rule says to use Acid Core flux for iron or mild steel. Mel Parrish Soldering Technology International Madison, AL 256 705 5530 256 705 5538 Fax [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Bev Christian Sent: Monday, October 22, 2001 11:34 AM To: [log in to unmask] Subject: Re: [TN] tin on iron and solder on iron OK, let me try saying this a different way: it "seems" that the canning industry has an easy time putting tin on can steel. Why do I have trouble getting solder to stick to a properly preheated 100% iron surface? Is it just a matter of flux strength? Or something else? Bev Christian Research in Motion -----Original Message----- From: Mel Parrish [mailto:[log in to unmask]] Sent: October 22, 2001 4:17 PM To: [log in to unmask] Subject: Re: [TN] tin on iron and solder on iron Dr Bev, Not sure what your question is but for discussion. Many of the common component lead frames contain significant amounts of iron which is plated to enhance solderability, limit corrosion, etc.. Seems that there should be some metallurgists out there that can lead us to understanding the solubility characteristics but my text books discuss FeSn intermetalics although the rate is slower that that of tin gold or tin copper. Also seems to me that the Nickel content is important to the solder interface. Mel Parrish Soldering Technology International 102 Tribble Drive Madison, AL 35758 256 705 5530 256 705 5538 Fax [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Bev Christian Sent: Friday, October 19, 2001 2:01 PM To: [log in to unmask] Subject: [TN] tin on iron and solder on iron OK, here is a general question for all you met guys. But I am not sure I can explain it well enough to be understood! We all know that tin can be put on iron or we wouldn't have "tin" cans. I also know it is difficult to put solder on iron. So my question is this: if one has a tinned iron surface and it is put into molten solder the tin will be dissolved into the molten solder. I presume when the piece of iron is withdrawn from the pot, solder will be well adhered to the iron. Is this because there is a solderable tin/iron intermetallic? What is the main difference between the tin can process and putting solder directly on iron that makes one easy to do and the other difficult? This may be a "first grade" met question, but I don't know the answer. Thanks. Bev Christian ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------