Terri, BT resin is made by Mitsubishi Gas Chemical Company, Inc. not Mitsui. Marion Graybeal ----- Original Message ----- From: Houston, Terri <[log in to unmask]> To: <[log in to unmask]> Sent: Monday, October 15, 2001 5:25 PM Subject: [TN] Mitsui's BN resin system > I'm looking for information on a board resin system that's supposed to have > a Tg around 300C. I was told it's the next generation of BT, made by Mitsui > and called BN. My web searches came up dry. > > If anyone has any leads on where I can find more information, I'd appreciate > it. > > Thanks, > Terri > > -------------------------------------------------------------------------- ------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > -------------------------------------------------------------------------- ------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------