I've had a similar thing happen in the past. I also use a 'layer build window' to allow a quick optical inspection of the bare boards. Just a clear area on the edge of the board with a number on each layer from 1 to n (this can include a revision code as well). You can hold the board up to the light and see the build from left to right through the board. It is possible to see the difference depths of the characters. I also include 'drawing number, issue, and layer' information on each layer, just outside of the board perimeter in fairly large (0.100") text to make things as clear as possible. (As well as the layer build diagram on my master drawing.) Another possibility, in addition, would be to include a small copper feature on each layer that gets exposed by the edge routing to indicate correct layup sequence. regards, Phil Dutton C.I.D. -----Original Message----- From: Speers, Samuel @ CSE [mailto:[log in to unmask]] Sent: Wednesday, 17 October 2001 6:13 To: [log in to unmask] Subject: Re: [TN] PCB layers swapped Genny, Don't know about electrical test, but practice at our site since Genesis 1:1 has been to design in a "window" where the pattern revision of each layer is visible. This enables you to see that the correct pattern rev. was used and that they are laid up in the correct order. Sam Speers -----Original Message----- From: Genny Gibbard [mailto:[log in to unmask]] Sent: Tuesday, October 16, 2001 1:07 PM To: [log in to unmask] Subject: [TN] PCB layers swapped Good morning, My morning has not been so good. I have a build of PCB's (over 300 boards) where two inner layers have been swapped. The board fabricator constructed the board in the wrong order. These boards are RF in nature and have frequencies approaching 2GHz on them. In many places we put a signal trace on the inner layer furthest from the component side and then a wide grounded trace over it on the closer inner layer as shielding. So not only is there no longer shielding over many traces, these signals are also about .03" closer to the component circuitry than they used to be. Can you contemplate the nightmare of spurious issues that have been created? We did not notice the problem until they were fully populated and almost thru our testing process and started failing one of the tests miserably. Needless to say, we will be revising our inspection techniques to try to catch occurrences like this much sooner. I was wondering if anyone knows of a way that layer order could be electrically tested for on a bare board, that we could require our fabricator to complete? Genny Gibbard (mailto:[log in to unmask]) ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------