Cathy, Because a few of the "icons" of the industry(Doug Pauls,etc.) tell you to. Unless you have a Freudian sense of humor,which can be attributed to drinking too much Mountain Dew(Doug Pauls,etc.),I believe you meant to say ionic wash. There are many reasons to clean an assembly,besides just removing flux or it's postreflow by-products.Knowing the end use enviroment,whether it is to be conformally coated,as well as many other factors will determine whether you need to clean after a no-clean process.If you would to talk to me off-line give me a call. Doug Pauls is also an excellent source of information. Dewey (602-436-2766) > -----Original Message----- > From: Cathy Killen [SMTP:[log in to unmask]] > Sent: Monday, July 30, 2001 5:50 AM > To: [log in to unmask] > Subject: [TN] Just a few Questions > > Hope someone can help. > Why is an 'iconic' wash required and is it required in a no-clean process? > Can a no-clean process achieve the desired standards, if not what is the > best way to achieve the standards? > Cathy Killen > Training Instructor > [log in to unmask] <mailto:[log in to unmask]> > An Oasis of Training Excellence > * 028 38314305 > > > > DISCLAIMER > 1. The information contained in this E-mail is confidential. > It is intended only for the stated addressee(s) and access to it by any > other person is unauthorised. > If you are not the addressee, you must not disclose, copy, circulate or in > any other way use or rely on the information contained in this E-mail. > Such > unauthorised use may be unlawful. If you believe that you have received > this E-mail in error, please inform us immediately and delete it and all > copies from your system. > 2. The views expressed in this E-mail are those of the author, and do > not represent the views of Smtek Europe., its associates or subsidiaries, > unless otherwise expressly indicated. In the avoidance of doubt, the > insertion of the name Smtek Europe., its associate or subsidiary under the > name of the sender may constitute an express indication that the views > stated in the Mail are those of the named company. > 3. Please note it is your responsibility to scan this E-mail for > viruses. > > -------------------------------------------------------------------------- > ------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET > Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > -------------------------------------------------------------------------- > ------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------