>>> <[log in to unmask]> 09/19/01 10:52AM >>> The Isol laminates web site has a few paper on this issue. http://www.isolalaminatesystems.com/technical/techpapers/index.htm IF anyone has additional info I would also be interested as well. Jack Crawford <[log in to unmask]>@IPC.ORG> on 09/18/2001 12:16:55 PM Please respond to "TechNet E-Mail Forum." <[log in to unmask]> Sent by: TechNet <[log in to unmask]> To: [log in to unmask] cc: Subject: Re: [TN] Via Reliability and Thermal Shock >>> "Buscomb, Scott" <[log in to unmask]> 09/18/01 11:10AM >>> I am looking for research on via reliability under thermal shock. I am particularly interested in drilled via (>200um). Is anyone aware of any papers, studies, etc? Thanks in advance, Scott Buscomb PCB Design Engineer Zight Corporation www.zight.com --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------