Ray I very strongly recommend the Vigon 200A from Dr Wack (the Zestron guys). It is a saponifier with a non-MEA but organic reactive molecule. It seems to be excellent in performance and possibly somewhat less smelly than the other organic saponifiers. It is a comparatively recent development, having been marketed for about 4 years. Brian "Golembiewski, Ray" wrote: > > I am using a Speedline Aquastorm 200 inline aqueous cleaner, and > would like to utilize this for removing RMA flux from my boards. I need > help determining what aqueous cleaner to use for this new process. > Please let me know what has worked for you, and possibly a contact name. > > Thanks, > > Ray Golembiewski C.I.D. > Manufacturing Test Engineer > Projects Unlimited, Inc. > (937) 918-2200 > > --------------------------------------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------