Franklin, I am evaluating Omikron Tin as well as Technic's Leveltech, Fidelity's 9099 and others, but I haven't yet evaluated FST. What is prompting you to switch from FST to Omikron? Why Omikron and not some of the other brands? Peter Blokhuis [log in to unmask] --- Franklin D Asbell <[log in to unmask]> wrote: > Howdy, > > It was decided to transition from Dexter/Enthone FST > to Florida Cirtech's Omikron, was wondering if > anyone out there has performed this already? And > what differences, learning curves, or adjustments > both minor and major we might expect. > > Thanks, > > Franklin D Asbell > Network Circuits, Inc. > Irving, Texas > http://www.networkcircuits.com > > __________________________________________________ Do You Yahoo!? Get email alerts & NEW webcam video instant messaging with Yahoo! Messenger http://im.yahoo.com --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------