Hi Ronny, Nickel and gold thickness in the barrel will and should be close to the same thickness as the nickel and gold thickness on the rest of the board. The mechanisms for corrosion are the same in a microvia as they are on the surface of the board, and varying the thickness would be impractical even if it wasn't. By the way, those thickness' are 100 to 200 micro inches of nickel and 3 to 5 micro inches of gold. Kind Regards Ryan Grant Advanced Technology Engineer MCMS (208) 898-1145 [log in to unmask] > -----Original Message----- > From: Ronald Rea [SMTP:[log in to unmask]] > Sent: Wednesday, September 26, 2001 2:37 PM > To: [log in to unmask] > Subject: [TN] Nickel/Gold in microvias > > Hello people of TechNet, > > What is the minimum nickel and gold thickness in the bottom of micro-vias. > IPC 6012 doesn't seem to be very specific on that point. > > On the surface, a minimum of 50 microinch seems sufficient, but how does > this garantee corrosion protection in the barrel of the blind vias? > > Your toughts please, > > Thanks, > > Ronny. > > > > > > _______________________________________________________ > Send a cool gift with your E-Card > http://www.bluemountain.com/giftcenter/ > > -------------------------------------------------------------------------- > ------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET > Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > -------------------------------------------------------------------------- > ------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------