We would either use
a jumper wire looped over the top of the QFP and soldered to both leads, or use
a short length of bare wire bridging the 2 leads. Wouldn't suggest a solder
bridge alone. You can see a little more about jumper wire on our web site at http://www.circuittechctr.com/guides/6-1.htm.
Jeff Ferry CEO Circuit Technology
Center, Inc www.circuittechctr.com [log in to unmask] 978-374-5000
-----Original Message----- From: David
Schaefer [mailto:[log in to unmask]] Sent: Wednesday, August 29, 2001
11:52 AM To:[log in to unmask] Subject: [TN] Rework
Specification
We have a fine pitch QFP which requires rework to short 2
adjacent pins. Is there a specification which outlines the requirements for
such rework? Is it acceptable to use a solder bridge rather than a jumper
wire?
Thanks,
Dave