Subject: Re: [TN] Solder TestingThis test should also be done at 500 deg F, not 480.T Reeves-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Monday, August 20, 2001 9:42 AM
Subject: Re: Solder TestingJ-STD-003 4.2.3.4.1 After fluxing and draining per . . . slide the coupon gently on molten solder. Allow coupon to float on solder for 5 seconds maximum. The coupon may be depressed into the solder bath to a maximum of 50% of the coupon thickness after it has been initially floated on the solder. After the elapsed time, slide the coupon off molten solder. Hold coupon still and horizontal until solder solidifies.Guy Ramsey
Senior Lab Technician / InstructorE-Mail: [log in to unmask]
Ph: (610) 362-1200 x107
Fax: (610) 362-1290-----Original Message-----Can someone tell me if there is a standard dwell time in a solder float test?
From: TechNet [mailto:[log in to unmask]]On Behalf Of Michael Lester
Sent: Monday, August 20, 2001 11:05 AM
To: [log in to unmask]
Subject: [TN] Solder Testing
2 inch square coupon using Kester Non-Activated flux,temperature of 480º
Thanks for the help.