Hallo, I'm making 12oz finished copper board as follows. 9x10inch 0.062inch CEM1 Single side Also currently making 4oz finished copper for the mass production. I don't see any problem for the backplane board with the belwo specified requirements. Please contact me if you have any questions...for these special boards. Thanks Johnnie -----Original Message----- From: <Peter George Duncan> [mailto:[log in to unmask]] Sent: Wednesday, August 08, 2001 11:37 AM To: [log in to unmask] Subject: Re: [TN] Leading Edge Supplier Search $)C Years ago (nearly 20) we used a Danish company called Printca to produce a thick (>0.25") 20 layer backplane for us. They were pretty leading edge at the time, as was the board. They still claim to be leading edge and you can find them at: Printca AS Postbox 8120 Svendborgvej 3 DK-9220 Aalborg (* DENMARK Phone: (+45) 99 30 2009 Fax: (+45) 99 30 9299 E-mail: [log in to unmask] Web: www.printca.dk Regards Pete Duncan "S. Miller" <CircuitekAsi To: [log in to unmask] [log in to unmask]> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group) Sent by: Subject: [TN] Leading Edge Supplier Search TechNet <[log in to unmask] ORG> 08/08/01 02:05 AM Please respond to "TechNet E-Mail Forum."; Please respond to CircuitekAsia Dear Comrades, I am in search of leading edge suppliers that can provide the following technologies: a. Backplane (multilayer; thickness ranging from .125-.250") b. Thick Cu technology (multilayer; ranging from 4oz to 6 oz) If anyone is aware of such a supplier(s), kindly advise name, and contact details if available. Your assistance and input is greatly appreciated. Regards, ------------------------------------------------------------------------ --------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509- 9700 ext.5315 ------------------------------------------------------------------------ ---------