The question you want to ask yourself is what do you want to measure? If you want to measure the placement accuracy of your placement machine then you will need to mount the inspection system pre reflow as there is no point mounting the system post reflow as the migration of the components will effect the results. You will need an AOI system that can offer a gauging capability. If you just want to inspect for component defects then again pre reflow would be better, as solder joint inspection causes the higher percentage of false calls on the AOI systems I have used. If you want the AOI system to complete a total inspection of components and solder joints then post reflow is the position for you. BUT you will need to buy a system which doesn't give you excessive false calls for solder quality and a system which can offer a short enough inspection cycle time so as not to become a bottleneck in your process, or a system that can complete a sample inspection on your product. It's a difficult decision to make, and this is coming from an engineer who used to work for an AOI manufacturer. Steve Brown praveen kumar manjeshwar wrote: > Hi everyone, > I just wanted to know where would it be preferable to postion an AOI > equipment on a production line. I have known of people who prefer to use it > before reflow and some who have suggested after reflow. > What would the implications be if this equipment is placed prior to and > after reflow? > Also, if one had to evaluate an AOI equipment (not solder paste measuring > equipments), then what factors would one have to consider to gage the > capability of this equipment? > Thanks > Praveen > > _________________________________________________________________ > Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp > > --------------------------------------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------