Hi Bill, looked at the pictures and re-read your description. Thought it was maybe reside from the solder mask. Are you using LPISM? But I'd expect no solder if there was mask residue present. Difficult without the boards in front of me. You could try a quick SEM-EDX analysis look for organic residue in the same areas on un-soldered boards. Of course that's only if residue looked to be an issue. If your OA flux worked then I doubt it'd be a residue issue, mask residue is a pretty robust substance. Best regards, Andrew Hoggan BBA Associates Ltd www.bba-associates.ltd -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Kasprzak, Bill (sys) USX Sent: 01 August 2001 13:35 To: [log in to unmask] Subject: [TN] Process Problem vs Board Problem Technetters' I've recently run into a problem with Wavesoldering some circuit boards where I am having problems getting topside solder joints. The process that I'm running has the topside of the board at 195-200 F just prior to the solder wave. My conveyor speed is 4.0 fpm. My fluxer is a spray fluxer. The board is a .062 - 6 layer board that has an aluminum heat sink on it. I feel that my process is set correctly. The original process that previously used on these boards was very successful when we used an OA water soluble flux. This process was on that I qualified many years ago to J-Std-001A for Class 3 assemblies. On these circuit boards, I'm trying to use a No Clean Lo Activity level flux that is water washable. Because I have new equipment for wavesoldering, I was hoping to not have to do a re-qualification process for our level 3 assemblies. Because our new equipment has much better controls than our old equipment I thought that it would be easy to solder these boards with an LO active flux. Well, my initial pass has been a disaster so far. There are three pictures that I'm looking for comments on. They are located on Steve's Webpage at http://stevezeva.homestead.com. (A thousand thanks go out to Steve Gregory for providing a site for posting the pictures.) Two of the pictures, called Bare Pad and Bare Pad2 show a condition that I can describe but I don't know if this condition has a name. In those pictures, there is a heavier coat of solder on the pad, but it seems to form a concentric ring on the pad.The extremities of the pads, both toward the outside and the inside, show a tinned surface but it appears to be much thinner. To me, it seems like these thin areas do not readily solder. It seems like this thin area is barrier that can only be overcome with a very strong OA flux. This may explain why I did not have a problem before. The other picture shows another condition that I see in various places on the bare board where there are protrusions on the inside of the PTH's. This appears to be trapped volitiles that were being expulsed during the HASL process. I'm trying to determine if I have a board problem or a process problem. Is it unreasonable for me to think that this board can be soldered with a no-clean (but water washable) LO activity level flux? Any help or comments would be greatly appreciated. Bill Kasprzak Moog Inc., Electronic Assembly Engineering ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------