Hi Tom, I must have missed your message last week. We offer X-ray services for BGAs as well as rework, materials and failure analysis work. Please contact me offline for more details and prices. As for BGA rework, we use a Conceptronics system (not sure of the model). For X-ray we use a XTEK HMX160 for manufacturing support and failure analysis work. This X-ray system has given us great service in the three years I have been here. Wade McFaddin Nextek Inc. > -----Original Message----- > From: Tom Parkinson - Quality System Manager [SMTP:[log in to unmask]] > Sent: Wednesday, August 08, 2001 2:13 PM > To: [log in to unmask] > Subject: Re: [TN] BGA and X-ray > > Kathy - I wrote practically the same question last week (I also asked > about outside services doing x-ray for BGA and average prices) - the > only replies were: check smta org in your area, one commercial site, and > one other person asking me to send him any answers I get. If you get > more info - please pass it on. > > Thanks > > > > Kathy Kuhlow wrote: > > > > Good Afternoon. Hope all is well with everyone. I was wondering, What > is the preferred equipment to use for BGA rework/replacement and xray? I > would like to know what equipment you are using and your likes/dislikes of > the equipment. > > > > TIA for all responses. > > > > Kathy > > > > > ------------------------------------------------------------------------ > > > > TEXT.htmName: TEXT.htm > > Type: Plain Text (text/plain) > > -------------------------------------------------------------------------- > ------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET > Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > -------------------------------------------------------------------------- > ------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------