hi, you got some really terrific suggestions. if i overlooked a similar response as mine, i apologize. what you need to be aware of is the importance of selecting a potting compound that won't shrink much during cure and that won't fracture during any temperature cycling that your potted assembly may be exposed to. stresses on potted magnetic components may change their performance. phil -----Original Message----- From: John Fahey [mailto:[log in to unmask]] Sent: Thursday, August 16, 2001 7:57 AM To: [log in to unmask] Subject: [TN] ''Encapsulating/Potting PCB Assemblies" I have recently come upon a requirement to encpasulate/pot a small PCB assy containing a T/H transformer. Size is approx .5"W x .5"L x .3" H Can anyone who has experience in "Potting" or "encapsulating" technologies ,especially potting PCB assemblies, give me some hints/starting points, etc. I would be very interested in any issues to watch out for, recommended potting materials, equipment, standards to adhere to, tests, etc. Basically anything that would be helpful. Thanks in advance, John --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------