Charlene -
 
Assuming you are going to do a manual breakaway of the boards, I recommend a final web thickness of 0.012" with 30 degree cutters on FR4. If you are using mechanical/machine separation you can go slightly thicker. The thin web thickness allows for easy, manual breakaway with minimal potential damage to the components and the solder joints.
 
I'm sorry but I have not used RF35 so I am not familiar with its physical characteristics. Ed/

Ed Valentine
Electronics Manufacturing Solutions
8612 Mourning Dove Road, Raleigh, NC 27615
Phone: (919) 270-5145, Fax: (919) 847-9971
Email: [log in to unmask]
Website: http://www.ems-consulting.com
----- Original Message -----
From: [log in to unmask] href="mailto:[log in to unmask]">Charlene Dwyer
To: [log in to unmask] href="mailto:[log in to unmask]">[log in to unmask]
Sent: Monday, August 06, 2001 8:01 PM
Subject: [DC] V Scoring

What depth, and angle do you spec on your panel drawings for scoring a board with a .062 thickness?

Does it make a difference on the Board Material because we are using a combination of FR4 and RF35 for a 4 layer board.

-Char