Hi Lou, We have our solder pot analysed once every three month, and the results have always (for more than 7 years) been within IPC-specifications. Although contamination-levels depend somewhat on conductor finishing and production volume, to my opinion your supplier is right. Kind regards, Daan Terstegge SMT Centre Thales Communications Unclassified mail Personal Website: http://www.smtinfo.net >>> Lou Hart <[log in to unmask]> 07/11 3:54 pm >>> TechNetters, I'd appreciate comments on contaminant analysis of a wave solder pot. We had been sending a sample out for analysis (type "C" I think it is, by the mil spec) once per month. Now the solder supplier is telling me that once every six months is more than enough. I've been taking the contaminant data and plotting Q charts (for short-run SPC the modern way, as I've been mentioning in this forum) with the monthly data. What has been your practice and recommendation? At the moment, it is hard for me to feel comfortable with a twice-yearly analysis of what seems to me to be an important material in our manufacturing process. Lou Hart --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------