"Pelkey, Glenn" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]> 07/25/01 06:10 AM
|
To: [log in to unmask] cc: Subject: [TN] Compression Strength Limit of FR-4 |
Here's one you don't get asked very often. What is the z-axis compression strength limit of FR-4? Not looking at Flexural Strength, unless you think there's a way of correlating the two.
Thanks,