hi,
all
the elements of a great test. simple, inexpensive, fast,
non-destructive.
thanks,
phil
WoW!
What a great picture of weave exposure. Would suggest that you
submit
this to the 600 and 610 groups for inclusion in those documents.
I was going to suggest that you can run a water soluble pen over
suspected
areas and if the glass is exposed the weave will wick up the ink
and when you
wipe it off with a tissue the result will be little colored
spots. If it is
merely texture there will be no spots.
Did
you notice this conditon prior to assembly?
Susan Mansilla
Robisan
Lab