Jorge If you can guarantee that it will be impossible for condensation to occur on the assembly, then it may be you could dispense with conformal coating. This can be done by not using a weatherproof/dust-tight box, but a hermetic one, and making sure that it is filled with a dry gas. Alternatively, you can heat the assemblies and any metalwork above them to about 10°C over ambient, so that any condensation will occur below the assemblies, where it can do no harm. You may find cleaning and coating the easiest solution, though. Brian Jorge Santana wrote: > > Hi > > I am not familiar to conformal coating process and I would like some > advice of using or not conformal coating in this specific application. > The board will located outside and should work properly for several years, > but will be enclosed inside a WEATHERPROOF and DUST-TIGHT box, this > condition is enough for not use conformal coating ? > Thanks for any advice. > > Jorge Santana > > --------------------------------------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------