Rob Try Loctite 7360 I had used and worked great http://www.loctite.com.hk/PRODUCTS/7360.htm Thanks Jorge Santana -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Rob Day Sent: Monday, June 18, 2001 7:09 AM To: [log in to unmask] Subject: [TN] Glue Nozzle Cleaning Hello Folks, We have some glue nozzles that are very dirty. We were wondering if there was a different way of cleaning them besides sending them out (called a couple of vendors but they would not quote site unseen) or spending money for a kit that may not work. Any input would be greatly appreciated. Thanks, Rob Day ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------