Peter, It is our experience that de-masking is easier with natural latex than synthetics which tend to break/fragment more easily. Regards, Graham Naisbitt [log in to unmask] www.concoat.co.uk <http://www.concoat.co.uk> For instant access to Product Data Sheets register on the Tech-Shot area of www.concoat.co.uk <http://www.concoat.co.uk> Concoat Limited Alasan House, Albany Park CAMBERLEY GU16 7PH UK Phone: +44 (0)1276 691100 Fax: +44 (0)1276 691227 Mobile: +44 (0)79 6858 2121 > -----Original Message----- > From: TechNet [mailto:[log in to unmask]]On Behalf Of Peter Swanson > Sent: Wednesday, June 13, 2001 04:53 > To: [log in to unmask] > Subject: Re: [TN] Ok conformal coating, but how ? > > > -----Original Message----- > From: Graham Naisbitt [mailto:[log in to unmask]] > Sent: 13 June 2001 15:33 > To: [log in to unmask] > Subject: Re: [TN] Ok conformal coating, but how ? > > >>Use a peelable latex temporary masking compound. Better results will > come > from a natural latex than a synthetic.<< > > Graham, > > Why? > > Peter > -- > ========================================================= > Peter Swanson [log in to unmask] > INTERTRONICS http://www.intertronics.co.uk > > INTERTRONICS is dedicated to providing quality material, > consumable and equipment solutions to the electronics > manufacturing and other technology based industries, with > the highest levels of technical support and customer > service. > > ------------------------------------------------------------------ > --------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following > message: SET Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & > Databases > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ------------------------------------------------------------------ > --------------- > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------