Happy Friday...and in Northern Ohio USA- welcome Mr. or Mrs. Sun!! We have just practiced processing .014 Pyralux pc bds. All went well until we had to solder mask the boards. We use a hand screened thermal cured mask. The boards are impossible because of warp factor. Does anyone out there know of a screening table with a vacuum to hold the boards in place for hand screening? Thanks. Mike