Jim It depends a) on the service conditions and b) the required reliability, as well as the factors mentioned by others. If you have a piece of, say, oil-prospecting instrumentation that fails in the middle of the Amazonian jungle and it requires 3 days of pirogue transport to the nearest helipad, 1 day to get it to an international airport, 15 days held up in customs, 2 days to get it back to you, 7 days to diagnose, repair the fault and test it and then the reverse transport procedure, just because you chose not to clean it, then it isn't going to do your company's reputation any good. My short answer is that if the goods are going to work under poor climatic conditions and you cannot afford a failure in the field, then you may start to believe that not cleaning could be inappropriate. That having been said, conformally coating over flux residues is ALWAYS potentially harmful to the health of a product and anyone who does it without a full risk assessment, based on a full series of both field and laboratory tests, must do so at his own risk. Even so, you cannot eliminate variables which can affect the results, such as a batch of bare boards which arrive in your plant with more hygroscopic contaminants on the surface than is usually the case and more than when you did the risk assessment. At your risk and perils... Brian "West, Jim" wrote: > > Hi, > > Do boards have to be cleaned before you apply conformal coating? Does it > depend on what type of flux is used? Example would be no-clean flux, you > can apply conformal coating over it right? > > Thanks, > Jim > > --------------------------------------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------