Hi Steve
Nice Blisters!
Microsections could tell you at what interface the delam occurred and that
might give you a clue.  I would include holes in the sections where you can.  
Wedge voids can
lead to such blisters if moisture is trapped at the interface.

Susan Mansilla
Robisan Lab