Steve, Maybe it's just me, but, while I can see the 2 x-sections, I don't have the x-rays. Earl, The die size and assembly process would be very helpful (attachment in vacuum?). While GaAs is a brittle material it will bend in 1.5 mil thickness' which is probably from TCE mismatch (obviously on larger die since the mismatches are not large) and I would think vac pressure could contribute as Steven suggested. Have you cross sectioned known good die to see if they are warped also? If the attachment voiding is significant, you might consider Ag epoxy attachment. With a thin bond line on a good Cu/Invar heat spreader like you have, 98% attachment with epoxy vs 60-70% with eutectic may be thermally acceptable, depending, of course, on your application. Also, you can check for cracks with a dye penetrant or often by slowly running a felt tip pen (like a red Flair) across the die while under a microscope. Capillary action will pull the ink into the crack(s) and obviously show it. Good Luck, Bruce Misner > ---------- > From: Stephen R. Gregory[SMTP:[log in to unmask]] > Reply To: TechNet E-Mail Forum.;[log in to unmask] > Sent: Wednesday, June 13, 2001 8:58 AM > To: [log in to unmask] > Subject: [TN] X-ray Images > > Hey ya'll! > > Earl has one more picture up, it's 4 x-ray images of the device showing > voiding under the die or thin eutectic. Go to: > > http://stevezeva.homestead.com/index.html > > Since he can't post from where he's at, he's asked me to pose the > following > question: > > "How much flexibility does GaAs have and is the current eutectic contour > too > much (as in x-sections on Steve's site)? Can these die crack under > additional > thermal stress and cause the catastrophic failures shown in other images?" > > > -Steve Gregory- > > > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------