low foaming water sol. solder mask?Charlie Are you sure it is not the wash chemistry that is reacting this way? My experience suggests that this is more likely. Regards, Graham Naisbitt [log in to unmask] www.concoat.co.uk Concoat Limited www.concoat.co.uk Alasan House, Albany Park CAMBERLEY GU16 7PH UK Phone: +44 (0)1276 691100 Fax: +44 (0)1276 691227 Mobile: +44 (0)79 6858 2121 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Charlie Pitarys Sent: Monday, May 21, 2001 03:16 To: [log in to unmask] Subject: [TN] low foaming water sol. solder mask? Can anyone recommend a low foaming w/s solder mask that does not cause foam to belch out of a batch dishwasher. I am cleaning rosin flux so a wash chemistry is needed. The current mask (includes a sodium compound)coupled with wash chemistry is causing severe foam. Thanks