In a message dated 5/14/01 3:38:10 PM US Eastern Standard Time, [log in to unmask] writes: << Can anyone tell me if there are any probblems using Electroless Nickel (5micron) / Immersion Gold (0.1 micron) as a surface finish on High Frequency boards (10GHz). Particularly,is nickel a poor conductor at High Frequencies? >> Gordon, I would call out the paper at IPC Expo last month in Anaheim, CA - "Effects of Surface Finish on High Frequency Signal Loss Using Substrate Materials". The paper reports that at 10 gigahertz, "thick" electroless nickel (200 microinch) shows a skin effect of about 0.9 dB/inch. This is more than for "thin" electroless nickel, OSP, immersion silver, and HASL. Table 1 in the article reports electroless nickel has 3-4X the resistance of eutectic solder and 30-40X the resistance of copper or silver. So, thicker electroless nickel, longer signal traces, and higher frequencies make the skin effect worse. Paper was joint between MacDermid, Taconic Laminates, Omni Circuits, and Rockwell Collins and received the "best technical paper" award at IPC Expo - 2001. The paper should be available through the IPC, or if publication is not pending, from one of the authors - I can refer you to one of them if you want an electronic copy. Dennis Fritz MacDermid, Inc Waterbury CT. --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------