Hi Jan! Steve G. posted the photo of your "stars" - my guess is that the star pattern is a "witness mark" which is due to a test probe leaving an indentation during electrical testing of the BGA component. The "stars" might be due to solidification shrinkage but typically surface physics does not behave in such a repeatable, crisp pattern! Ask your BGA supplier if they conduct electrical test on the BGA components. Good Luck. Dave Hillman Rockwell Collins [log in to unmask] "Pelchat, Janice" <[log in to unmask]>@IPC.ORG> on 05/02/2001 07:26:24 AM Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to "Pelchat, Janice" <[log in to unmask]> Sent by: TechNet <[log in to unmask]> To: [log in to unmask] cc: Subject: [TN] Seeing STARS! (BGA solderball anomaly) We have some ceramic BGAs that are giving us problems with fractures at the ball/package interface after reflow. In the process of failure analysis, we inspected unassembled parts under high power and have seen two anomalies. One is an apparent shaving of the outside perimeter balls from what appears to be fixturing at the manufacturer - that is being F/Ad by the manufacturer. The other anomaly is what I can only term a "star" shaped appearance on the surface of the solderballs. Under very high power, this "star" effect seems (to me at least) to be the result of the solidification process of the solderball during manufacture. It looks as though the solder surface separated - then the separations formed crevices in a star pattern. Think of the appearance of crevices formed on crusty breads when they bake and cool. (Sorry for the analogy - in my other life - I bake). I have a fair picture for those wanting to see a visual. Does this sound familiar to anyone? Is it part of the normal BGA solderball appearance? Jan Pelchat Benchmark Electronics --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------