hi, we thin it with mek to a sprayable viscosity. phil -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Tuesday, May 22, 2001 9:57 AM To: [log in to unmask] Subject: [TN] solithane conf. coat I hope this one gets though. First thanks to all for the help you have given and the education I receive from the Technet. I have trouble responding in kind, our e-mail doesn't always let me reply. Now the question. Does anyone spray Solithane 113 conformal coat? We are currently brushing with it, but I have been asked to spray. Is there any special info I should know? We spray manually with a paint gun or an airbrush. Thanks again ( especially my last question- soldering to stainless steel ) Fortunately I won't have to do that after all. Charles Caswell Process Lead, PCB Frontier Electronic Systems --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------