It is not the chemistry, by itself it has about zero foam. Boards from the surface mount line clean without foam occuring, i.e. no w/s mask. It even foamed with a competing brand. Foaming is only seen when boards from the wave solder line w/gobs of w/s mask applied are run. The incoming water is hot. Bottom line is the one constituant in the mask, Sodium Salt of Polymeric Carboxylic Acid, combine this with rosin flux and you get the StaPuff marshmellow monster from ghost busters. So I know whats causing it, I'm just looking for what others are using and not seeing these issues. Thanks -----Original Message----- From: Graham Naisbitt [mailto:[log in to unmask]] Sent: Monday, May 21, 2001 12:32 PM To: TechNet E-Mail Forum.; Charlie Pitarys Subject: RE: [TN] low foaming water sol. solder mask? Charlie Are you sure it is not the wash chemistry that is reacting this way? My experience suggests that this is more likely. Regards, Graham Naisbitt [log in to unmask] www.concoat.co.uk Concoat Limited www.concoat.co.uk <http://www.concoat.co.uk/> Alasan House, Albany Park CAMBERLEY GU16 7PH UK Phone: +44 (0)1276 691100 Fax: +44 (0)1276 691227 Mobile: +44 (0)79 6858 2121 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Charlie Pitarys Sent: Monday, May 21, 2001 03:16 To: [log in to unmask] Subject: [TN] low foaming water sol. solder mask? Can anyone recommend a low foaming w/s solder mask that does not cause foam to belch out of a batch dishwasher. I am cleaning rosin flux so a wash chemistry is needed. The current mask (includes a sodium compound)coupled with wash chemistry is causing severe foam. Thanks