In the very early 1960s, I had this problem with a Fry's Flowsolder machine (I think it was the first soldering machine to be put into service in Switzerland). This machine had a fixed speed pump motor and a sort of butterfly valve for controlling wave height. I put a geared down DC motor on the valve shaft and fixed two insulated titanium rods (about 2 mm diameter) onto the conveyor guide. One rod was about 1.5 mm longer than the other. A relay was connected to each rod, so that it was activated when the rod was earthed (grounded) by contact with the wave. If the long rod was not grounded, the motor was activated to open the valve slowly until it was grounded. If both were grounded, the motor closed the valve until the top rod was not touching the solder. This always held the wave to the correct height, no matter the volume of solder, the temperature, the position or angle of the conveyor, the power voltage/frequency etc. It worked OK for 12 years until that machine was definitively replaced, used mostly on boards 0.8 mm thick. I can recollect only one occasion when solder overflowed the top surface of the board, probably due to a sudden power surge, upping the solder level before the controller could react. I don't think we ever had solder skipping, except when a board had been incorrectly placed in the pallet. Simple, cheap and effective. In the case where the pump motor speed controls the wave height, a similar system changing the speed could be easy to install. FWIW Brian "Rougeux, Scott" wrote: > > Good Afternoon, > > I am interested in products or companies that can offer me a resolution for > closed loop control of wave solder heights. Years ago I used to use a > product called an AccuWave...is there anything out there similar to > this................ > > tanks > > --------------------------------------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------