Kathie: We use Chemtronics Flux-Off CZ. We use the material judiciously due to its high cost but works extremely well. We have a process where we use the material to clean connectors that we pre-tinned using RMA flux. We also use aerosol spray cans to clean difficult areas. We perform touch up and secondary operations with RMA fluxes. Use of this material is limited to Class 3 hardware. Bill Kasprzak Moog Inc. > -----Original Message----- > From: Lambert, Katherine A. [SMTP:[log in to unmask]] > Sent: Wednesday, March 07, 2001 11:10 AM > To: [log in to unmask] > Subject: [TN] Bench top cleaning of hand soldering > > Hi folks, > > We're in the process of looking for a solvent to replace the Axarel 2200 > and > IPA that we are using for flux removal at hand soldering operations. We > are > using RMA flux cored solder and RMA external flux. We have mostly the > standard types of surface mount parts and connectors on organic CCAs. > Nothing terribly exotic - just the basics. > > What are you folks using out there in TechNet land? > > Thanks, > > Kathie Lambert > SMT Process Engineer > Northrop Grumman > Baltimore, MD > 410-765-9746 > > -------------------------------------------------------------------------- > ------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send the following message: SET > Technet NOMAIL > Search previous postings at: www.ipc.org > On-Line Resources & Databases > > E-mail Archives > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > -------------------------------------------------------------------------- > ------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------