hi, try j-std-002, paragraph 4.2.2 (test b). see also figure 5. that might work. phil -----Original Message----- From: peter lee [mailto:[log in to unmask]] Sent: Wednesday, March 21, 2001 4:30 PM To: [log in to unmask] Subject: [TN] 0402 Solderability Test Hello, Does anyone know if there is any industry standard method for testing solderability of 0402 chip caps? I am also interested in knowing if there is any specs. that will apply. Thank you. Peter __________________________________________________ Do You Yahoo!? Get email at your own domain with Yahoo! Mail. http://personal.mail.yahoo.com/ --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------