I have taken some pic for the problem I mentioned in last email. The board is a single sided board, with wave soldering. I hope the Technet will accept this email with the zip file attacted to it. Thanks for the supports you guys had been giving me in this. Rudolph ------Original Message------ From: Werner Engelmaier <[log in to unmask]> To: [log in to unmask] Sent: March 28, 2001 8:24:08 PM GMT Subject: Re: [TN] BGA crack- major headache Hi Rudolph, I think you have too complex a situation to get a proper diagnosis to your problem via the TechNet forum. We need to see a good picture(s) showing the failure mode, we need to see details of the BGA construction as well as the PCB, and also get some idea of any testing (ESS, burn-in) you have performed on your product prior to shipping. Further, the use conditions are critical. Werner Engelmaier Engelmaier Associates, L.C. Electronic Packaging, Interconnection and Reliability Consulting 7 Jasmine Run Ormond Beach, FL 32174 USA Phone: 386-437-8747, Fax: 386-437-8737 E-mail: [log in to unmask], Website: www.engelmaier.com --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------