Yes it is a reject, a fracture is a fracture. How could you assure that the fracture wouldn't continue to get worse over time? Another thought, how can you be assured that what you see is actually the full extent of the issue? Kathy >>> [log in to unmask] 02/27/01 09:56AM >>> Hi Technetters, It is stated in IPC-A-610C that a fractured joint is considered defect in all classes. Can anyone confirm that it would be the same if the fracture is on the component side? And why should it be considered as defect if the joint on the secondary side is good. Would the fracture extend from the primary side to the secondary side? Thanks in advance... JF WABTEC CORPORATION CONFIDENTIALITY NOTE The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited.