Good Afternoon,
I am looking for some input as far as what is
the highest the top side temperature can be on a pcb going over the wave solder
before there is damage (bonding) to components (ex: transistors, IC's etc). Any
help would be appreciated. We are seeing around 254 degrees F
Thanks in advance,