Grant,
I briefly worked for a small company that used these little guys extensively, with repeated failures. I could not get them designed out. They (caps) absolutely do not like washing and we had problems with some no-clean pastes even. It would appear the structure/chemistry of these things makes them sponges. Whether that leads specifically to delamination I cannot say.
Bev Christian
Research in Motion
-----Original Message-----
From: Grant Emandien [mailto:[log in to unmask]]
Sent: February 22, 2001 9:44 AM
To: [log in to unmask]
Subject: [TN]
Hi,
Has anyone experienced delaminating of glued PPS chip capacitors?
Regards
Grant
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------