Hi everyone! My problem today has to do with stencils for solder paste printing. We are having a lot of problems with the glue releasing when we go to use the stencil. Packing tape will hold through the end of the job. The temperature is OK and the time in cleaner is acceptable according to the stencil vendor. We have checkout our stencil cleaner and the parameters on the various printers. We have had our stencil cleaner for many years and only had the problem in the last year.' We have had no luck with the problem and the stencil vendor is also confused. Has anyone had this problem before and found a solution? Tenison Stone Telex Communications --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------