Hi Rudy! Good information but Doug and I are looking for something more specific - would you expect the DI water to increase the oxide thickness of the aluminum bond pads or attack/remove material on the aluminum bond pads? And if the attack/remove scenario is selected, how deep of an attack? Angstroms or microinches in depth? The exposures we are dealing with is room temperature and a maximum of 60 minutes exposure duration. Dave Hillman Rockwell Collins [log in to unmask] "<Rudy Sedlak>" <[log in to unmask]>@IPC.ORG> on 02/03/2001 05:57:46 PM Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to [log in to unmask] Sent by: TechNet <[log in to unmask]> To: [log in to unmask] cc: Subject: Re: [TN] DI water and aluminum bond pads In hopes of bringing just a LITTLE bit of chemistry to this discussion.... Pure water is not inherently more corrosive....it is probably less so, HOWEVER, Pure water lacks buffering power, the pH moves easily if anything affects it, the impurities, and especially water hardness, are pH buffers. And so, when atmospheric Carbon Dioxide (which is an acid gas, forming carbonic acid when it reacts with water) hits water which has no buffering power, the pH falls like a rock. Further, when water is purified by deionization, acid (H+) is introduced in the cation column to replace the metals removed from the solution, and Hydoxide (OH-) is introduced in the anion column, and if there is a SLIGHT imbalance, the pH can swing widely. And last, oxide-free Aluminum is actually attacked by pure, neutral water. But we never see true oxide-free Aluminum. Aluminum depends on its insoluble oxide coat for protection, and if the pH gets even slightly acid or base, that coating starts becoming soluble....and you got attack. So, PLEASE stop saying pure water attacks Aluminum. Pure water will not dissolve the oxide coat, so you do not get attack. Actually truly pure water, at pH 7 (which is the pH of truly pure water) would not attack Aluminum, because it would not dissolve the oxide coating, but obtaining such a critter (pure water) in the real world is just about impossible. I will go away quietly now. Rudy Sedlak---who tries to avoid even drinking pure water RD Chemical Company --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------